Mi-Tech Metals Super Chatter Freeâ„¢ HD17.7 Tungsten-Based Metal

Category Metal , Nonferrous Metal , Refractory Metal , Tungsten Alloy
Manufacturer Mi-Tech Metals
Trade Name Super Chatter Free™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mi-Tech Metals Super Chatter Freeâ„¢ HD17.7 Tungsten-Based Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE which combine to resist thermal fatigue. The high melting point reduces soldering or erosion problems. To increase the machinability of this brittle metal, alloying elements are added and practical use of tungsten is possible for die casting tools.Used in resistance brazing and high temp applications. Used as counter weights and counter balances, radiation shielding components, tool shanks for boring bars and other tools for chatter-free machining.Data provided by Mi-Tech Metals.
Physical Properties Metric English Comments
Density 17.7 g/cc
0.639 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 34
34
Tensile Strength, Ultimate 862 MPa
125000 psi
Tensile Strength, Yield 655 MPa

@Strain 0.200 %
95000 psi

@Strain 0.200 %
Elongation at Break 4.0 %
4.0 %
in 50 mm
Modulus of Elasticity 365 GPa
52900 ksi
Thermal Properties Metric English Comments
CTE, linear 4.50 µm/m-°C

@Temperature 20.0 - 400 °C
2.50 µin/in-°F

@Temperature 68.0 - 752 °F
Thermal Conductivity 113 W/m-K
784 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Ni, Fe, Mo 7.0 %
7.0 %
Tungsten, W 93 %
93 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000120 ohm-cm
0.0000120 ohm-cm