Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000170 ohm-cm | 0.0000170 ohm-cm | |
Hogen HM1100 Tungsten-Based Metal Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers hig.. |
|||
Electrical Resistivity | 0.0000170 ohm-cm | 0.0000170 ohm-cm | |
Mi-Tech Metals HD17D Tungsten-Based Metal Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; ASTM B-777-07 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Slightly Magnetic.Manufactured by powder metallurgy methods. The t.. |
|||
Electrical Resistivity | 0.0000170 ohm-cm | 0.0000170 ohm-cm | |
Indium Corp. Indalloy 130 Tin-Lead Solder Alloy Inexpensive utility solderInformation Provided by Indium Corporation |
|||
Electrical Resistivity | 0.0000170 ohm-cm | 0.0000170 ohm-cm | 3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02 |
California Fine Wire Nickel 211 (Nickel Manganese Alloy) All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |