Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000540 ohm-cm | 0.0000540 ohm-cm | |
TIMET CP Titanium (ASTM Grade 3) Commercially Pure Titanium. Industry Specifications: USA Aerospace: AMS 4900. Germany Aerospace: 3.7055. France: T-50. UK Aerospace Specification DTD 5023, 5273.Features: The mechanical properti.. |
|||
Electrical Resistivity | 0.0000540 ohm-cm | 0.0000540 ohm-cm | |
Bohler-Uddeholm BÖHLER S601 (M2 Modified) High Speed Steel For Cold Work Applications Properties: Tungs ten-molybdenum high speed steel with ex cel lent toughness and cut ting proper ties, for a wide variety of uses.Applications: Taps, twist drills, reamers, broaching tools, meta.. |
|||
Electrical Resistivity | 0.0000540 - 0.0000560 ohm-cm | 0.0000540 - 0.0000560 ohm-cm | |
AK Steel DI-MAX® HF-10 Nonoriented Electrical Steel DI-MAX HF-10 is a fully processed nonoriented electrical steel designed for use in high speed motors, traction motors, aircraft generators, and other rotating equipment operating at frequencies abov.. |