Electrical Properties Metric English Comments
Electrical Resistivity 0.00007917 ohm-cm
0.00007917 ohm-cm
AK Steel 11 Cr-Cb™ Ferritic Stainless steel
AK Steel 11 Cr-Cb™ has increased silicon levels and is dual stabilized with titanium and columbium. Designed for use in automotive exhaust tubing and other high-temperature applications, this is a..