Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0001075 ohm-cm | 0.0001075 ohm-cm | |
Special Metals INCONEL® Alloy MA 754 A mechanically alloyed nickel-chromium alloy with oxide dispersion strengthening. Mechanical alloying, which involves high-energy milling of metal powders, is used to create a uniformly distributed.. |