Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000109 ohm-cm | 0.000109 ohm-cm | |
Special Metals NIMONIC® Alloy 75 A nickel-chromium alloy with good mechanical properties and oxidation resistance at high temperatures. Used for sheet-metal fabrications in gas-turbine engines, for components of industrial furnace.. |
|||
Electrical Resistivity | 0.000109 ohm-cm | 0.000109 ohm-cm | Temperature Factor is 1.04 at 800°C (1470°F). Temperature Factor is 1.05 at 1000°C (1830°F). Temperature Factor is 1.07 at 1200°C (2190°F). |
Resistalloy International Resistalloy 8020 Nickel Chromium Electrical Resistance Alloy Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at.. |