Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Electrical Resistivity = 0.000110 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.000110 ohm-cm
0.000110 ohm-cm
HP Alloys Nitronic® 50 Austenitic Stainless, Annealed
Annealed applies to tensile, impact, and hardness values and are for 3/4 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of co..
Electrical Resistivity 0.000110 ohm-cm
0.000110 ohm-cm
HP Alloys Nitronic® 50 Austenitic Stainless, Level 2 Cold Worked
Cold Worked applies to tensile values and are for 0.25 to 4 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion resis..
Electrical Resistivity 0.000110 ohm-cm
0.000110 ohm-cm
HP Alloys Nitronic® 50 Austenitic Stainless, Level 3 Cold Worked
Cold Worked applies to tensile values and are for 0.25 to 2.4 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion res..
Electrical Resistivity 0.000110 ohm-cm
0.000110 ohm-cm
HP Alloys Nitronic® 50 Austenitic Stainless, Level 4 Cold Worked
Cold Worked applies to tensile values and are for 1/4 to 2 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion resist..
Electrical Resistivity 0.000110 ohm-cm
0.000110 ohm-cm
Temperature coefficient of resistance is 180 µOhm/Ohm-°C in the range 25-500°C.
Special Metals BRIGHTRAY® Alloy B Electrical Resistance Alloy
A nickel-iron-chromium electrical-resistance alloy for use at operating temperatures up to 2010°F (1100°C). It contains rare-earth additions for increased oxidation resistance, especially und..
Electrical Resistivity 0.000110 ohm-cm
0.000110 ohm-cm
Temperature coefficient of resistance is 60 µOhm/Ohm-°C in the range 25-500°C.
Special Metals BRIGHTRAY® Alloy S Electrical Resistance Alloy
A nickel-chromium electrical-resistance alloy for use at temperatures up to 2100°F (1150°C) under continuous operating conditions. It is similar to BRIGHTRAY alloy C but does not contain rare..
Electrical Resistivity 0.000110 ohm-cm
0.000110 ohm-cm
Special Metals NIMONIC® Alloy PE16
A precipitation-hardenable nickel-iron-chromium alloy with an addition of molybdenum for solid-solution strengthening. It has good strength and oxidation resistance at temperatures to about 1380°..
Electrical Resistivity 0.000110 ohm-cm
0.000110 ohm-cm
HP Alloys Nitronic® 50 Austenitic Stainless, Level 1 Cold Worked
Cold Worked applies to tensile values and are for 0.25" to 4" diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion resistanc..
Electrical Resistivity 0.000110 ohm-cm
0.000110 ohm-cm
HP Alloys Nitronic® 50 Austenitic Stainless, Level 5 Cold Worked
Cold Worked applies to tensile values and are for 0.25 to 1.5 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion resis..