Special Metals BRIGHTRAY® Alloy S Electrical Resistance Alloy

Category Metal , Electronic/Magnetic Alloy , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Special Metals (includes the former Inco Alloys International Inc.)
Trade Name BRIGHTRAY®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Special Metals BRIGHTRAY® Alloy S Electrical Resistance Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A nickel-chromium electrical-resistance alloy for use at temperatures up to 2100°F (1150°C) under continuous operating conditions. It is similar to BRIGHTRAY alloy C but does not contain rare-earth additions. It has good resistance to oxidizing, neutral, and reducing atmospheres. The alloy has a low temperature coefficient of resistance. Used for heating elements in industrial furnaces. The standard product forms are strip and wire.Data provided by the manufacturer, Special Metals.
Physical Properties Metric English Comments
Density 8.43 g/cc
0.305 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 735 MPa
107000 psi
Annealed
Thermal Properties Metric English Comments
CTE, linear 12.5 µm/m-°C

@Temperature 20.0 - 500 °C
6.94 µin/in-°F

@Temperature 68.0 - 932 °F
Specific Heat Capacity 0.419 J/g-°C
0.100 BTU/lb-°F
Melting Point 1400 - 1420 °C
2550 - 2590 °F
Solidus 1400 °C
2550 °F
Liquidus 1420 °C
2590 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.15 %
<= 0.15 %
Chromium, Cr 19 - 21 %
19 - 21 %
Iron, Fe <= 1.0 %
<= 1.0 %
Manganese, Mn <= 2.5 %
<= 2.5 %
Nickel, Ni 75 %
75 %
Including Cobalt, calculated as remainder
Silicon, Si 0.75 - 1.75 %
0.75 - 1.75 %
Sulfur, S <= 0.010 %
<= 0.010 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.000110 ohm-cm
0.000110 ohm-cm
Temperature coefficient of resistance is 60 µOhm/Ohm-°C in the range 25-500°C.