Electrical Resistivity 0.000116 ohm-cm

@Temperature 100 °C
0.000116 ohm-cm

@Temperature 212 °F
Haynes 263® alloy, cold rolled sheet, solution treated and aged
Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle..
Electrical Resistivity 0.000116 ohm-cm
0.000116 ohm-cm
Special Metals INCONEL® HX Nickel Superalloy
Data provided by the manufacturer, Special Metals.
Electrical Resistivity 0.000116 ohm-cm

@Temperature 659 °C
0.000116 ohm-cm

@Temperature 1220 °F
AK Steel 304 Austenitic Stainless steel
AK Steel 304 is a variation of the basic 18-8 grade, Type 302. Lower carbon, in Type 304, minimizes chromium carbide precipitation due to welding and its susceptibility to intergranular corrosion. ..
Electrical Resistivity 0.000116 ohm-cm

@Temperature 659 °C
0.000116 ohm-cm

@Temperature 1220 °F
AK Steel 304L Austenitic Stainless steel
AK Steel 304L is an extra low-carbon variation of Type 304, that eliminates carbide precipitation due to welding. AK Steel 304L can be used in the "as-welded" condition, even in severe corrosive co..
Electrical Resistivity 0.000116 ohm-cm
0.000116 ohm-cm
ATI Allegheny Ludlum Stainless Steel Ohmaloy® 40 Resistance Alloy
Ohmaloy 40 alloy is a moderately magnetic, ductile stainless steel having extremely high electrical resistivity. In addition to imparting high electrical resistivity, the aluminum content in these ..
Electrical Resistivity 0.000116 ohm-cm
0.000116 ohm-cm
Special Metals INCONEL® Alloy HX
A nickel-chromium-iron-molybdenum alloy with outstanding strength and oxidation resistance at temperatures to 2200°F (1200°C). Matrix stiffening provided by the molybdenum content results in high..