Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | <= 0.000200 ohm-cm | <= 0.000200 ohm-cm | |
Lord Adhesives 6144 Silver Conductor LORD 6144 silver conductor is a one-component, thermosetting conductive epoxy designed for surface mount attachment of electronic component devices. It is primarily used as a chip-to-lead frame adhe.. |
|||
Electrical Resistivity | 0.000200 ohm-cm | 0.000200 ohm-cm | |
Epoxyset Epoxiohm EO-30FST Electrically Conductive Epoxy Adhesive EO-30-FST is two part, fast cure, silver filled, and high electrical conductivity epoxy adhesive. Both components are silver filled permitting a simple 1:1 mix ratio by weight. It has smooth creamy .. |