Material Notes:
EO-30-FST is two part, fast cure, silver filled, and high electrical conductivity epoxy adhesive. Both components are silver filled permitting a simple 1:1 mix ratio by weight. It has smooth creamy consistency. It can cure in 4 to 8 hours at room temperature.Information provided by Epoxyset Inc.
Physical Properties Metric English Comments
Density 3.10 g/cc
0.112 lb/in³
Viscosity >= 50000 cP
>= 50000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D >= 70
>= 70
ASTM D2240
Shear Strength 12.0 MPa
1740 psi
Adhesive Bond Strength 9.65 MPa
1400 psi
Lap Shear Strength
Thermal Properties Metric English Comments
CTE, linear 72.0 µm/m-°C
40.0 µin/in-°F
Thermal Conductivity 2.00 W/m-K
13.9 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Glass Transition Temp, Tg >= 40.0 °C
>= 104 °F
Electrical Properties Metric English Comments
Electrical Resistivity 0.000200 ohm-cm
0.000200 ohm-cm
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 40.0 °C
1.00 hour

@Temperature 104 °F
480 - 720 min

@Temperature 25.0 °C
8.00 - 12.0 hour

@Temperature 77.0 °F
Pot Life 10 min
10 min