Polymer Property : Electrical Resistivity = 1.35e+11 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 1.35e+11 - 2.68e+12 ohm-cm
1.35e+11 - 2.68e+12 ohm-cm
Average value: 9.78e+11 ohm-cm Grade Count:12
Overview of materials for Phenolic, Novolac, Heat Resistant Grade, Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Heat Resistant Grade, Filled". Each property range of values reported is minimum and ..
Electrical Resistivity 1.35e+11 ohm-cm
1.35e+11 ohm-cm
ASTM D257
Plenco 4246 Phenolic, Granular, Injection Molded  (discontinued **)
Two-stage Phenolic. PLENCO 04246 flow 18 is a black two-stage, medium heat resistant phenolic molding compound. It has excellent electrical, moldability and molded finish characteristics. It is use..