Polymer Property : Electrical Resistivity = 1.40e+17 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 1.40e+17 ohm-cm
1.40e+17 ohm-cm
per ASTM D257-91
DuPont™ Kapton® 300HN Polyimide Film, 75 Micron Thickness
Film thickness 75 micron (3.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).General..
Electrical Resistivity 1.40e+17 ohm-cm
1.40e+17 ohm-cm
per ASTM D257-91
DuPont™ Kapton® 300VN Polyimide Film, 75 Micron Thickness
Film thickness 75 micron (3.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type HN with added dimensional stability. Available i..
Electrical Resistivity 1.40e+17 ohm-cm
1.40e+17 ohm-cm
DuPont™ Kapton® 120FN616 Polyimide/FEP Composite Film
120 Gauge film structure consisting of a 25 µm (1 mil) base polyimide film with a 2.5 µm (0.1 mil) coating of Teflon® FEP on both sides.Kapton® Type HN film coated with Teflon® FEP fluoropolyme..