Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.50 ohm-cm | 1.50 ohm-cm | Through Thickness |
GrafTech eGRAF® HITHERM™ HT-2505 Graphite with Polymer Additive Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Electrical Resistivity | 1.50 ohm-cm | 1.50 ohm-cm | Through Thickness |
GrafTech eGRAF® HITHERM™ HT-2510 Graphite with Polymer Additive Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Electrical Resistivity | 1.50 ohm-cm | 1.50 ohm-cm | Through Thickness |
GrafTech eGRAF® HITHERM™ HT-705 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Electrical Resistivity | 1.50 ohm-cm | 1.50 ohm-cm | Through Thickness |
GrafTech eGRAF® HITHERM™ HT-710 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Electrical Resistivity | 1.50 ohm-cm | 1.50 ohm-cm | Through Thickness |
GrafTech eGRAF® HITHERM™ HT-720 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Electrical Resistivity | 1.50 ohm-cm | 1.50 ohm-cm | Through Thickness |
GrafTech eGRAF® HITHERM™ HT-1205 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Electrical Resistivity | 1.50 ohm-cm | 1.50 ohm-cm | Through Thickness |
GrafTech eGRAF® HITHERM™ HT-1210 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Electrical Resistivity | 1.50 ohm-cm | 1.50 ohm-cm | Through Thickness |
GrafTech eGRAF® HITHERM™ HT-1220 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |