Electrical Resistivity 2.00e+13 - 1.50e+16 ohm-cm
2.00e+13 - 1.50e+16 ohm-cm
Average value: 3.68e+15 ohm-cm Grade Count:18
Overview of materials for Cyanoacrylate Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr..
Electrical Resistivity 1.00e+12 - 1.50e+16 ohm-cm
1.00e+12 - 1.50e+16 ohm-cm
Average value: 6.25e+15 ohm-cm Grade Count:4
Overview of materials for Polyetherimide (PEI), 40% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 40% Glass Fiber". Specific grades with glass content between 35% and 44% are included. E..
Electrical Resistivity 1.00e+7 - 1.50e+16 ohm-cm

@Temperature 75.0 - 300 °C
1.00e+7 - 1.50e+16 ohm-cm

@Temperature 167 - 572 °F
Average value: 3.36e+15 ohm-cm Grade Count:2
Overview of materials for Epoxy Cure Resin
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M..