Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 2.00e+13 - 1.50e+16 ohm-cm | 2.00e+13 - 1.50e+16 ohm-cm | Average value: 3.68e+15 ohm-cm Grade Count:18 |
Overview of materials for Cyanoacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Electrical Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® BR111BL is a glass and mineral filled polyphenylene sulfide compounds developed to provide a good combination of mechanical strength and electrical proper.. |
|||
Electrical Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Ryton® R-7-120NA Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-7-120NA is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good weldline strength and low maintenance moldi.. |
|||
Electrical Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-7-120BL is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good weldline strength and low maintenance molding using.. |
|||
Electrical Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | IEC 93 |
Solvay Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH50 Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Technyl A 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical prope.. |
|||
Electrical Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | |
Covestro Desmopan® 460 Thermoplastic Polyurethane Desmopan 460 is a TPU on the basis of a special ester.Applications: Bearing shells, gear wheels, seals, cable connectors.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience w.. |
|||
Electrical Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | |
Arkema Group Rilsan® BZM 23 G9 Nylon 11, 23% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA11,MS,18-040,(G+C)(F+D)(25+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Additive free.Rigidity. Low fric.. |
|||
Electrical Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® BR111 is a glass and mineral filled polyphenylene sulfide compounds developed to provide a good combination of mechanical strength and electrical .. |