Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 150 - 1.63e+16 ohm-cm | 150 - 1.63e+16 ohm-cm | Average value: 1.63e+15 ohm-cm Grade Count:102 |
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va.. |