Electrical Properties Metric English Comments
Electrical Resistivity 3.50e+13 ohm-cm
3.50e+13 ohm-cm
ASTM D257
Shell Carilon® DP R1000 Polyketone  (discontinued **)
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP R1000 is a high flow developmental engineering polyketone resin from Shell Chemi..