Polymer Property : Electrical Resistivity = 4.09e+12 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 4.09e+12 ohm-cm
4.09e+12 ohm-cm
ASTM D257
Plenco Valite 697-A Novolac Phenolic, Granular, Compression Molded  (discontinued **)
This Valite product has been replaced by Plenco 7697. Data provided by Plenco.VALITE 697-A is a black, two stage, improved impact phenolic molding compound. It has been specifically formulated for ..