Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 4.50e+12 ohm-cm | 4.50e+12 ohm-cm | Insulation Resistance; Recovery, 24 hrs after 10-day Cycling (25°C, 50% Relative Humidity) |
Cytec Conathane® CC-1194 (Conap) Polyurethane Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |
|||
Electrical Resistivity | 4.50e+12 ohm-cm | 4.50e+12 ohm-cm | Insulation Resistance; Recovery, 24 hrs after 10-day Cycling (25°C, 50% Relative Humidity) |
Cytec Conathane® CE-1164 (Conap) Polyurethane Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |