Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+14 - 4.50e+16 ohm-cm | 1.00e+14 - 4.50e+16 ohm-cm | Average value: 8.94e+15 ohm-cm Grade Count:12 |
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum .. |