Polymer Property : Electrical Resistivity = 4.50e+16 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 - 4.50e+16 ohm-cm
1.00e+14 - 4.50e+16 ohm-cm
Average value: 8.94e+15 ohm-cm Grade Count:12
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum ..