Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 4400 ohm-cm | 4400 ohm-cm | |
BASF Sicotan® Yellow K 1010 Color Additive Chemical Structure: Ni/Sb/Ti-oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA, PETP, CA/CAB and UPRecommendations for food applications: B.. |
|||
Electrical Resistivity | 4400 ohm-cm | 4400 ohm-cm | |
BASF Sicotan® Yellow K 2011 Color Additive Chemical Structure: Cr/Sb/Ti-oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA, PETP, CA/CAB and UPRecommendations for food applications: B.. |