BASF Sicotan® Yellow K 2011 Color Additive

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer BASF
Trade Name Sicotan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Sicotan® Yellow K 2011 Color Additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemical Structure: Cr/Sb/Ti-oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA, PETP, CA/CAB and UPRecommendations for food applications: BgVV, FDA, FrancePhysical form: PowderInformation provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.700 g/cc
0.0253 lb/in³
Density 4.50 g/cc
0.163 lb/in³
pH 7.0 - 8.0
7.0 - 8.0
Specific Surface Area 5.0 m²/g
5.0 m²/g
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 320 °C
608 °F
Electrical Properties Metric English Comments
Electrical Resistivity 4400 ohm-cm
4400 ohm-cm
Descriptive Properties Value Comments
Chemical Fastness (months) H2SO4 10%
>6 months
H2SO4 conc.
>6 months
HCI 10%
>6 months
HCI conc.
>6 months
HNO3 10%
>6 months
HNO3 conc.
3 months
Na2CO3 sat.
>6 months
NaOH conc.
>6 months
Color Yellow
Light Fastness 8
Migration Fastness 5