Polymer Property : Electrical Resistivity = 5.9566e+17 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 5.9566e+17 ohm-cm
5.9566e+17 ohm-cm
ASTM D257
Plenco 50130 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 50130 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in natural and black.Informat..