Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0500 - 50.0 ohm-cm | 0.0500 - 50.0 ohm-cm | |
MarkeTech Silicon Single Crystal Semiconductor Wafer, p-type, Boron Doped, Czochralski-LED Grown Data provided by the supplier, MarkeTech International.MarkeTech International supplies standard silicon single crystals grown with diameters from 51 to 150 mm from polycrystal material with donor c.. |
|||
Electrical Resistivity | 5.00 - 50.0 ohm-cm | 5.00 - 50.0 ohm-cm | ASTM D257 |
PolyOne Edgetek® NI-40CF/000 Nylon 6/10 - 40% Carbon Fiber Reinforced
(discontinued **) Data provided by PolyOne. |