Polymer Property : Electrical Resistivity = 5.00 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 5.00 - 3.39e+14 ohm-cm

@Temperature 50.0 - 50.0 °C
5.00 - 3.39e+14 ohm-cm

@Temperature 122 - 122 °F
Average value: 4.04e+13 ohm-cm Grade Count:19
Overview of materials for PVC, Flexible Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Flexible Grade". Each property range of values reported is minimum and maximum values of appropriat..
Electrical Resistivity 5.00 - 3.00e+17 ohm-cm
5.00 - 3.00e+17 ohm-cm
Average value: 4.97e+15 ohm-cm Grade Count:117
Overview of materials for Epoxy Encapsulant, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o..
Electrical Resistivity 5.00 - 1.00e+14 ohm-cm
5.00 - 1.00e+14 ohm-cm
Average value: 1.11e+13 ohm-cm Grade Count:10
Overview of materials for Nylon 610, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of..
Electrical Resistivity 5.00 - 200 ohm-cm
5.00 - 200 ohm-cm
MarkeTech Silicon Single Crystal Semiconductor Wafer, p-type, Dopant: NDT, Float Zone Grown
Data provided by the supplier, MarkeTech International.MarkeTech International supplies standard silicon single crystals grown with diameters from 51 to 150 mm from polycrystal material with donor c..
Electrical Resistivity 5.00 - 50.0 ohm-cm
5.00 - 50.0 ohm-cm
ASTM D257
PolyOne Edgetek® NI-40CF/000 Nylon 6/10 - 40% Carbon Fiber Reinforced  (discontinued **)
Data provided by PolyOne.
Electrical Resistivity 5.00 - 1.00e+9 ohm-cm
5.00 - 1.00e+9 ohm-cm
Average value: 7.19e+7 ohm-cm Grade Count:15
Overview of materials for Polypropylene with Carbon Black Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v..