Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 6.00e+14 ohm-cm | 6.00e+14 ohm-cm | ASTM D257 |
Rostone Rosite® 3950ES SMC Thermoset Polyester, 25% Glass Reinforced