Electrical Properties Metric English Comments
Electrical Resistivity 6.00e+14 ohm-cm
6.00e+14 ohm-cm
ASTM D257
Rostone Rosite® 3950ES SMC Thermoset Polyester, 25% Glass Reinforced  (discontinued **)
Key Features: High Strength; High DielectricElectrical grade material that provides higher flexural and impact strength than Rosite 3550 composites with comparable glass fiber content. 3950ES is fo..