Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 6.00e+15 ohm-cm | 6.00e+15 ohm-cm | ASTM D257 |
Plaskolite PETG Mirror Sheet Versatile fabrication properties with good impact strength, good design flexibility, and speed of fabrication.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Electrical Resistivity | 6.00e+15 ohm-cm | 6.00e+15 ohm-cm | ASTM D257 |
Chevron Phillips Ryton® R10 5004A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Electrical Resistivity | 6.00e+15 ohm-cm | 6.00e+15 ohm-cm | 40 hours at 23°C, 50% RH; ASTM D257 |
PTS Tristar® PC-10FRN (V) 15 MFI, 5VA, Flame Retardant, UV Stabilized Polycarbonate With Release ROHS Compliant.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Electrical Resistivity | 6.00e+15 ohm-cm | 6.00e+15 ohm-cm | Compound; ASTM D257 |
Borealis Casico™ FR4807 Non-Halogen Flame Retardant Compound for Low Voltage Insulation and Jacketing Casico FR4807 is a natural, thermoplastic polyolefin compound designed for flame retardant low voltage wire insulation and jacketing. As such, FR4804 offers a unique combination of good extrusion pr.. |
|||
Electrical Resistivity | 6.00e+15 ohm-cm | 6.00e+15 ohm-cm | ASTM D257 |
Ascend Performance Materials VYDYNE® 21SP Nylon, General Purpose 1.4% Deformation under 14 MPa (2000 psi) load.Typical property data. VYDYNE is a registered trademark of Solutia Inc. |