Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 6.00e+9 - 1.70e+14 ohm-cm | 6.00e+9 - 1.70e+14 ohm-cm | Average value: 9.82e+12 ohm-cm Grade Count:19 |
Overview of materials for Phenolic, Novolac, Impact Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Impact Grade, Filled". Each property range of values reported is minimum and maximum .. |
|||
Electrical Resistivity | 6.00e+9 ohm-cm | 6.00e+9 ohm-cm | ASTM D257 |
Plenco 7021 Black Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok 7021 is the replacement material for the former Union Carbide BMRS-7021. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of.. |
|||
Electrical Resistivity | 6.00e+9 ohm-cm | 6.00e+9 ohm-cm | ASTM D257 |
Plaslok 7021 Black Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 7021 is the replacement material for .. |