Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 7021 Black Impact Grade Phenolic Molding Compound  (discontinued **)

Category Polymer , Thermoset , Phenolic , Phenolic, Novolac, Impact Grade, Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 7021 Black Impact Grade Phenolic Molding Compound  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Plaslok 7021 is the replacement material for the former Union Carbide BMRS-7021. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of switchgear parts, or where mechanical assembly requires better impact strength.Data provided by Plaslok Corporation.Plaslok Corporation was purchased by Plastics Engineering Company in March 2000. The Plaslok name is no longer used on any products.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Apparent Bulk Density 0.480 g/cc
0.0173 lb/in³
ASTM D1895
Water Absorption 0.50 %
0.50 %
ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
Compression; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 41.0 MPa
5950 psi
ASTM D638
Flexural Yield Strength 74.0 MPa
10700 psi
ASTM D790
Flexural Modulus 6.90 GPa
1000 ksi
ASTM D790
Compressive Yield Strength 228 MPa
33100 psi
ASTM D695
Izod Impact, Notched 0.240 J/cm
0.450 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 171 °C
340 °F
ASTM D648
UL RTI, Electrical 150 °C

@Thickness 1.57 mm
302 °F

@Thickness 0.0618 in
UL RTI, Mechanical with Impact 150 °C

@Thickness 1.57 mm
302 °F

@Thickness 0.0618 in
UL RTI, Mechanical without Impact 150 °C

@Thickness 1.57 mm
302 °F

@Thickness 0.0618 in
Flammability, UL94 V-0

@Thickness 3.18 mm
V-0

@Thickness 0.125 in
V-0

@Thickness 3.18 mm
V-0

@Thickness 0.125 in
Electrical Properties Metric English Comments
Electrical Resistivity 6.00e+9 ohm-cm
6.00e+9 ohm-cm
ASTM D257
Dielectric Constant 4.5

@Frequency 1e+6 Hz
4.5

@Frequency 1e+6 Hz
ASTM D150
6.0

@Frequency 60 Hz
6.0

@Frequency 60 Hz
ASTM D150
Dielectric Strength 11.8 kV/mm
300 kV/in
ASTM D149
Dissipation Factor 0.040

@Frequency 1e+6 Hz
0.040

@Frequency 1e+6 Hz
ASTM D150
0.11

@Frequency 60 Hz
0.11

@Frequency 60 Hz
ASTM D150
Comparative Tracking Index 125 V
125 V
UL 746
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved