Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 6.38e+10 - 2.13e+12 ohm-cm | 6.38e+10 - 2.13e+12 ohm-cm | Average value: 5.65e+11 ohm-cm Grade Count:7 |
Overview of materials for Phenolic, Novolac, Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Flock Filled". Each property range of values reported is minimum and maximum values o.. |