Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.100 - 6.70e+17 ohm-cm | 0.100 - 6.70e+17 ohm-cm | Average value: 2.85e+16 ohm-cm Grade Count:351 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |