Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.100 - 1.00e+10 ohm-cm | 0.100 - 1.00e+10 ohm-cm | Average value: 2.95e+8 ohm-cm Grade Count:60 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Electrical Resistivity | 0.100 - 1.00e+16 ohm-cm | 0.100 - 1.00e+16 ohm-cm | Average value: 7.69e+15 ohm-cm Grade Count:13 |
Overview of materials for Styrenic TPE
(Unverified Data**) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic TPE". Each property range of values reported is minimum and maximum values of appropriate MatWe.. |
|||
Electrical Resistivity | 0.100 - 1.00e+14 ohm-cm | 0.100 - 1.00e+14 ohm-cm | Average value: 4.62e+13 ohm-cm Grade Count:13 |
Overview of materials for Acetal Copolymer, Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Electrical Resistivity | 0.100 - 1000 ohm-cm | 0.100 - 1000 ohm-cm | Average value: 258 ohm-cm Grade Count:27 |
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Electrical Resistivity | 0.100 - 1.00e+12 ohm-cm | 0.100 - 1.00e+12 ohm-cm | Average value: 1.58e+10 ohm-cm Grade Count:64 |
Overview of materials for Polycarbonate, Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val.. |
|||
Electrical Resistivity | 0.100 ohm-cm - 1e+05 | 0.100 ohm-cm - 1e+05 | Average value: 1160 ohm-cm Grade Count:17 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Electrical Resistivity | 0.100 - 1.00e+8 ohm-cm | 0.100 - 1.00e+8 ohm-cm | Average value: 1260 ohm-cm Grade Count:45 |
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Electrical Resistivity | 0.100 - 1.00e+8 ohm-cm | 0.100 - 1.00e+8 ohm-cm | Average value: 4.37e+6 ohm-cm Grade Count:26 |
Overview of materials for Nylon 612, Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Carbon Fiber Filler". Each property range of values reported is minimum and maximum values of.. |
|||
Electrical Resistivity | 0.100 - 10.0 ohm-cm | 0.100 - 10.0 ohm-cm | Average value: 5.39 ohm-cm Grade Count:4 |
Overview of materials for Nylon 11 + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp.. |
|||
Electrical Resistivity | 0.100 - 25.0 ohm-cm | 0.100 - 25.0 ohm-cm | |
MarkeTech Silicon Single Crystal Semiconductor Wafer, n-type, Phosphorous Doped, Czochralski-LED Grown Data provided by the supplier, MarkeTech International.MarkeTech International supplies standard silicon single crystals grown with diameters from 51 to 150 mm from polycrystal material with donor c.. |
|||
Electrical Resistivity | <= 0.100 ohm-cm | <= 0.100 ohm-cm | specific resistance |
Imerys Kaolexâ„¢ SC Kaolin Kaolex SC is an air floated Hydrated Aluminum Silicate. It is a low surface area, low viscosity, medium casting filler/extender for ceramic applications.Information provided by Imerys |
|||
Electrical Resistivity | 0.100 ohm-cm | 0.100 ohm-cm | Through-Plane |
GrafTech eGRAF® SPREADERSHIELD™ SS600 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Electrical Resistivity | 0.100 - 1.00 ohm-cm | 0.100 - 1.00 ohm-cm | ASTM C611 |
Techmer ES Electrafil® DB-1200/S/7/FR ABS, 7% Stainless Steel Fiber Reinforced (dry blend), Flame Retardant Superior cost-performance when compared with other electrically conductive resins is a hallmark of Electrafil stainless steel fiber reinforced ABS. Electrafil compounds can be formulated to meet UL.. |
|||
Electrical Resistivity | 0.100 - 1.00 ohm-cm | 0.100 - 1.00 ohm-cm | ASTM C611 |
Techmer ES Electrafil® DB-1200/SS/7 ABS, 7% Stainless Steel Fiber Reinforced (dry blend) Superior cost-performance when compared with other electrically conductive resins is a hallmark of Electrafil stainless steel fiber reinforced ABS. Electrafil compounds can be formulated to meet UL.. |
|||
Electrical Resistivity | 0.100 ohm-cm | 0.100 ohm-cm | Specific Resistance |
UBE Tyranno Grade H Ceramic Semi-Conductive Fiber Description: Tyranno Fiber is the continuous ceramic fiber consisting of Si, Ti or Zr,C and O. Advanced composites reinforced by the Tyranno Fiber are expected to play a very important role in the e.. |
|||
Electrical Resistivity | 0.100 - 0.500 ohm-cm | 0.100 - 0.500 ohm-cm | Specific resistance |
UBE Tyrannohex® Heat Resistant Composite Description: Tyrannohex is a fiber assembled ceramic with both toughness like a shell or wood and excellent heat-resistance in air.Very high volume fraction (Vf) of the thin (~ 10m), continuous fibe.. |
|||
Electrical Resistivity | <= 0.100 ohm-cm | <= 0.100 ohm-cm | ASTM D1829 |
CoorsTek Pure SiC™ LR CVD Silicon Carbide, > 99.9995% Data Provided by the manufacturer, CoorsTek, Inc. |
|||
Electrical Resistivity | 0.100 - 1.00 ohm-cm | 0.100 - 1.00 ohm-cm | |
A. Schulman ComAlloy Comshield® 229 ABS, Electrically Conductive - Stainless Steel Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Electrical Resistivity | 0.100 - 10.0 ohm-cm | 0.100 - 10.0 ohm-cm | Average value: 6.70 ohm-cm Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS), NCG Fiber This property data is a summary of similar materials in the MatWeb database for the category "PPS + NGG". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Electrical Resistivity | 0.100 - 1.00e+10 ohm-cm | 0.100 - 1.00e+10 ohm-cm | Average value: 2.94e+8 ohm-cm Grade Count:35 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo.. |
|||
Electrical Resistivity | 0.100 - 6.70e+17 ohm-cm | 0.100 - 6.70e+17 ohm-cm | Average value: 2.85e+16 ohm-cm Grade Count:351 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |