Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | >= 1000 V @Temperature 90.0 - 90.0 °C |
>= 1000 V @Temperature 194 - 194 °F |
Average value: 7220 V Grade Count:9 |
Overview of materials for Phenolic, Novolac, Fabric Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Fabric Filled". Each property range of values reported is minimum and maximum values .. |
|||
Dielectric Breakdown | >= 1000 V @Time 20.0 - 60.0 sec |
>= 1000 V @Time 0.00556 - 0.0167 hour |
Average value: 7220 V Grade Count:9 |
Overview of materials for Phenolic, Novolac, Fabric Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Fabric Filled". Each property range of values reported is minimum and maximum values .. |
|||
Dielectric Breakdown | >= 1000 V @Temperature 90.0 °C, Time 20.0 sec |
>= 1000 V @Temperature 194 °F, Time 0.00556 hour |
Step-by-step test, In oil, parallel to laminations; IEC 1212-2 5.1 |
Hippe PF CC 42 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical and electrical applications. Coarse weave (18 to 30 threads per cm).Information provided by Hippe. |
|||
Dielectric Breakdown | >= 1000 V @Temperature 90.0 °C, Time 60.0 sec |
>= 1000 V @Temperature 194 °F, Time 0.0167 hour |
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1 |
Hippe PF CC 42 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical and electrical applications. Coarse weave (18 to 30 threads per cm).Information provided by Hippe. |
|||
Dielectric Breakdown | >= 1000 V @Temperature 90.0 °C, Time 20.0 sec |
>= 1000 V @Temperature 194 °F, Time 0.00556 hour |
Step -by-step test, In oil, parallel to laminations; IEC 1212-2 5.1 |
Hippe PF CC 43 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical and electrical applications. Very coarse weave (less than 18 threads per cm).Information provided by Hippe. |
|||
Dielectric Breakdown | >= 1000 V @Temperature 90.0 °C, Time 60.0 sec |
>= 1000 V @Temperature 194 °F, Time 0.0167 hour |
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1 |
Hippe PF CC 43 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical and electrical applications. Very coarse weave (less than 18 threads per cm).Information provided by Hippe. |