Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Breakdown = 1000 V Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Breakdown >= 1000 V

@Temperature 90.0 - 90.0 °C
>= 1000 V

@Temperature 194 - 194 °F
Average value: 7220 V Grade Count:9
Overview of materials for Phenolic, Novolac, Fabric Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Fabric Filled". Each property range of values reported is minimum and maximum values ..
Dielectric Breakdown >= 1000 V

@Time 20.0 - 60.0 sec
>= 1000 V

@Time 0.00556 - 0.0167 hour
Average value: 7220 V Grade Count:9
Overview of materials for Phenolic, Novolac, Fabric Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Fabric Filled". Each property range of values reported is minimum and maximum values ..
Dielectric Breakdown >= 1000 V

@Temperature 90.0 °C,
Time 20.0 sec
>= 1000 V

@Temperature 194 °F,
Time 0.00556 hour
Step-by-step test, In oil, parallel to laminations; IEC 1212-2 5.1
Hippe PF CC 42 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod
Used in mechanical and electrical applications. Coarse weave (18 to 30 threads per cm).Information provided by Hippe.
Dielectric Breakdown >= 1000 V

@Temperature 90.0 °C,
Time 60.0 sec
>= 1000 V

@Temperature 194 °F,
Time 0.0167 hour
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1
Hippe PF CC 42 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod
Used in mechanical and electrical applications. Coarse weave (18 to 30 threads per cm).Information provided by Hippe.
Dielectric Breakdown >= 1000 V

@Temperature 90.0 °C,
Time 20.0 sec
>= 1000 V

@Temperature 194 °F,
Time 0.00556 hour
Step -by-step test, In oil, parallel to laminations; IEC 1212-2 5.1
Hippe PF CC 43 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod
Used in mechanical and electrical applications. Very coarse weave (less than 18 threads per cm).Information provided by Hippe.
Dielectric Breakdown >= 1000 V

@Temperature 90.0 °C,
Time 60.0 sec
>= 1000 V

@Temperature 194 °F,
Time 0.0167 hour
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1
Hippe PF CC 43 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod
Used in mechanical and electrical applications. Very coarse weave (less than 18 threads per cm).Information provided by Hippe.