Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 53000 V @Thickness 1.57 mm |
53000 V @Thickness 0.0620 in |
Cond A; ASTM D229 S/S |
Industrial Laminates/Norplex NP193M Synthetic Fabric Base Grade Description: 17 oz. aramide and “soft glass†fibers are combined to make a fabric that is stronger than pure aramide and less abrasive than glass fabrics. This material is impregnated with.. |
|||
Dielectric Breakdown | 53000 V @Thickness 1.57 mm |
53000 V @Thickness 0.0620 in |
Cond A; ASTM D229 S/S |
Industrial Laminates/Norplex NP634 Laminate Description: Warm punching, composite grade with woven glass covers for improved flexural, tensile and impact strength. Electrical properties comparable to NP611.Thickness Tested: 0.062", 0.125" and.. |