Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | <= 0.0020 ohm | <= 0.0020 ohm | Initial Surface Resistivity (SR) |
Parker Chomerics CHO-FOIL CCE Shielding Tape Conductive Adhesive Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or ti.. |
|||
Surface Resistance | <= 0.0020 ohm @Temperature 85.0 °C, Time 605000 sec |
<= 0.0020 ohm @Temperature 185 °F, Time 168 hour |
(SR); CHO-TP-57 |
Parker Chomerics CHO-FOIL CCE Shielding Tape Conductive Adhesive Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or ti.. |
|||
Surface Resistance | <= 0.0020 ohm | <= 0.0020 ohm | Initial Surface Resistivity (SR); CHO-TP-57 |
Parker Chomerics CHO-FOIL CCH Shielding Tape Conductive Adhesive Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or ti.. |
|||
Surface Resistance | <= 0.0020 ohm | <= 0.0020 ohm | Initial Surface Resistivity (SR); CHO-TP-57 |
Parker Chomerics CHO-FOIL CCJ Shielding Tape Conductive Adhesive Aluminum FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or .. |
|||
Surface Resistance | <= 0.0020 ohm | <= 0.0020 ohm | Initial Surface Resistivity (SR); CHO-TP-57 |
Parker Chomerics CHO-FOIL CCK Shielding Tape Conductive Adhesive Tin-plated Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, alum.. |
|||
Surface Resistance | <= 0.0020 ohm | <= 0.0020 ohm | Initial through resistivity (TR); CHO-TP-57 |
Parker Chomerics CHO-FOIL CCK Shielding Tape Conductive Adhesive Tin-plated Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, alum.. |
|||
Surface Resistance | <= 0.0020 ohm @Temperature 85.0 °C |
<= 0.0020 ohm @Temperature 185 °F |
95% RH; (SR); CHO-TP-57 |
Parker Chomerics CHO-FOIL CCK Shielding Tape Conductive Adhesive Tin-plated Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, alum.. |
|||
Surface Resistance | <= 0.0020 ohm @Temperature 85.0 °C |
<= 0.0020 ohm @Temperature 185 °F |
95% RH; (TR); CHO-TP-57 |
Parker Chomerics CHO-FOIL CCK Shielding Tape Conductive Adhesive Tin-plated Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, alum.. |
|||
Surface Resistance | <= 0.0020 ohm @Temperature 85.0 °C, Time 605000 sec |
<= 0.0020 ohm @Temperature 185 °F, Time 168 hour |
(SR); CHO-TP-57 |
Parker Chomerics CHO-FOIL CCK Shielding Tape Conductive Adhesive Tin-plated Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, alum.. |
|||
Surface Resistance | <= 0.0020 ohm @Temperature 85.0 °C, Time 605000 sec |
<= 0.0020 ohm @Temperature 185 °F, Time 168 hour |
(TR); CHO-TP-57 |
Parker Chomerics CHO-FOIL CCK Shielding Tape Conductive Adhesive Tin-plated Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, alum.. |
|||
Surface Resistance | <= 0.0020 ohm @Temperature 121 °C, Time 605000 sec |
<= 0.0020 ohm @Temperature 250 °F, Time 168 hour |
(SR); CHO-TP-57 |
Parker Chomerics CHO-FOIL CCK Shielding Tape Conductive Adhesive Tin-plated Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, alum.. |
|||
Surface Resistance | <= 0.0020 ohm @Temperature 121 °C, Time 605000 sec |
<= 0.0020 ohm @Temperature 250 °F, Time 168 hour |
(TR); CHO-TP-57 |
Parker Chomerics CHO-FOIL CCK Shielding Tape Conductive Adhesive Tin-plated Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, alum.. |
|||
Surface Resistance | <= 0.0020 ohm @Time 605000 sec |
<= 0.0020 ohm @Time 168 hour |
Salt fog corrosion; (SR); CHO-TP-57 |
Parker Chomerics CHO-FOIL CCK Shielding Tape Conductive Adhesive Tin-plated Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, alum.. |
|||
Surface Resistance | <= 0.0020 ohm @Time 605000 sec |
<= 0.0020 ohm @Time 168 hour |
Salt fog corrosion; (TR); CHO-TP-57 |
Parker Chomerics CHO-FOIL CCK Shielding Tape Conductive Adhesive Tin-plated Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, alum.. |