Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
PolyOne Bergamid™ A70 white Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | ASTM D257 |
RTP Company PermaStat® 1800A FR Polycarbonate/Acrylic Alloy (PC/PMMA) Anti-Static - Flame Retardant Anti-Static - Flame RetardantComments:Permanently Anti-StaticESD ProtectionFlame RetardantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect p.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+16 ohm | 1.00e+10 - 1.00e+16 ohm | Average value: 1.45e+15 ohm Grade Count:23 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
Surface Resistance | <= 1.00e+10 ohm | <= 1.00e+10 ohm | |
Lehmann & Voss LUVOCOM® 1105-8264 PEEK, with CNT Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect.. |
|||
Surface Resistance | >= 1.00e+10 ohm | >= 1.00e+10 ohm | |
Lehmann & Voss LUVOCOM® 1105-8451 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio.. |
|||
Surface Resistance | >= 1.00e+10 ohm | >= 1.00e+10 ohm | |
Lehmann & Voss LUVOCOM® 3-8266/BL Polyamide 6, unreinforced Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
Solvay TECHNYL® C 216 V35 Black Z PA6, 35% glass fiber, Conditioned Description: Polyamide PA6 , reinforced with 35 % of glass fiber, for injection molding.Available in: North AmericaProduct Applications: It has good mechanical properties, it is used in all sectors .. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
Solvay TECHNYLSTARâ„¢ S 216 V30 PA6, 30% glass filled, Conditioned Description: TECHNYL STAR TM Polyamide, reinforced with 30% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific, Europe and North AmericaPr.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
Techmer ES Electrablend® ABS CF5 5% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 5% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Surface Resistance | 1e+05 - 1.00e+10 ohm | 1e+05 - 1.00e+10 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DDF029 PC LNP STAT-KON* DDF029 is a compound based on Polycarbonate resin containing Carbon, Glass Fiber. Added features of this material include: Electrically Conductive. Flame Retardant. |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY P3000U PA 6 (Europe-Africa-Middle East) LNP* Stat-loy* P3000U is a compound based on PA 6 resin. Added features include; Antistatic, UV - Stabilized. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
Polyram PlusTek PB826G3 Nylon 6 for Injection Molding, 15% Glass-fiber Reinforced, Impact Modified and UV Stabilized 15% Glass fiber reinforced, impact modified and UV stabilized Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | ISO 3915 |
CP-Polymer-Technik Wellamid® 6000 GS 40 HWCP 40% Glass Sphere Filled Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | ISO 3915 |
CP-Polymer-Technik Wellamid® 6000 MR 309 HWCP Mineral Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | ISO 3915 |
CP-Polymer-Technik Wellamid® 6600 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | ISO 3915 |
CP-Polymer-Technik Wellamid® 6600 TLWCP Nylon 66, Flame Protection Grade V-2, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
EMS-Grivory Grivory® TSGZ-15/4 PA666-GF15 Information provided by EMS Grivory |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
EMS-Grivory Grivory® XE 4176 black 9288 PA1010-GF50 Product description: Grilamid XE 4176 black 9288 is a 50% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4176 black 9288 are: PA1010.. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Conditioned) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Surface Resistance | 1.00e+10 - 3.16e+10 ohm | 1.00e+10 - 3.16e+10 ohm | IS 3396-1979 |
Amity Thermosets ATM 144 Phenolic Molding Organic Filler, Compression Molded Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane.. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Conditioned) Ultramid A3EG3 is a 15% glass fiber reinforced injection molding PA66 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Conditioned) Ultramid A3X2G7 is a 35% glass fiber reinforced injection molding PA66 grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stif.. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
BASF Ultramid® A3XZG5 BK 23187 25% Glass Filled PA66 FR (Conditioned) Description: Impact-modified, 25% glass-fiber reinforced injection-molding grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; for compone.. |
|||
Surface Resistance | 1.00e+10 - 3.16e+10 ohm | 1.00e+10 - 3.16e+10 ohm | IS 3396-1979 |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Compression Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft/medium flow Applications:Telecommuni.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+16 ohm | 1.00e+10 - 1.00e+16 ohm | Average value: 5.72e+14 ohm Grade Count:40 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | ASTM D257 |
RTP Company PermaStat® 2700-50A Stryrenic Thermoplastic Elastomer (TES) Anti-Static - Shore 50 A
&am Anti-Static - Shore 50 AComments:Permanently Anti-StaticESD Protection50-A DurometerUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect propert.. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Conditioned) Ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase.. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Conditioned) Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | |
LATI Laticonther 62 CEG/500-V0HF1 PA 6, Glass/Mineral Reinforced, Flame Retardant High thermal conductivity product based on Polyamide 6 (PA6). Glass fibers / Mineral filler. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Mid.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+13 ohm | 1.00e+10 - 1.00e+13 ohm | Average value: 4.31e+12 ohm Grade Count:35 |
Overview of materials for Nylon 6, Cast This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |