Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.20e+7 ohm | 1.20e+7 ohm | Dry; ASTM D257 |
Westlake Plastics Lennite® SD-P UHMW-PE (static dissipative) Carbon-powder filled, self-lubricating, moisture-repellent material with resistivity levels in the 10^5-10^9 range. This material has the highest impact strength, is lightweight, has excellent abra.. |