Electrical Properties Metric English Comments
Surface Resistance 1.30e+15 ohm
1.30e+15 ohm
ASTM D257
Arkema Group Orgalloy® RS 6030 Polyamide 6 Alloy 30% Glass Fiber reinforced
Polyamide Alloy, Rigid grade, Nylon 6 basedMolding of Engineering PartsInformation provided by Arkema Group