Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+14 - 1.50e+14 ohm | 1.00e+14 - 1.50e+14 ohm | ASTM D257 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Asia Pacific) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Surface Resistance | 1.00e+14 - 1.50e+14 ohm | 1.00e+14 - 1.50e+14 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Asia Pacific) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Surface Resistance | 1.00e+14 - 1.50e+14 ohm | 1.00e+14 - 1.50e+14 ohm | ASTM D257 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Surface Resistance | 1.00e+14 - 1.50e+14 ohm | 1.00e+14 - 1.50e+14 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Surface Resistance | 1.00e+14 - 1.50e+14 ohm | 1.00e+14 - 1.50e+14 ohm | ASTM D257 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Europe-Africa-Middle East) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Surface Resistance | 1.00e+14 - 1.50e+14 ohm | 1.00e+14 - 1.50e+14 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Europe-Africa-Middle East) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |