Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 2.30e+14 ohm | 2.30e+14 ohm | 50% RH, 500V; ASTM D257 |
ALM PA-616-GS Filled Nylon 12 Prototyping Polymer 50% glass sphere filled material for improved dimensional stability, increased stiffness, and higher temperature applications when compared to unfilled PA.The PA 616-GS can be processed on any laser.. |
|||
Surface Resistance | 2.30e+14 ohm | 2.30e+14 ohm | 50% RH, 500V; ASTM D257 |
ALM PA 614-GS Filled Nylon 12 Prototyping Polymer 40% glass sphere filled material for improved dimensional stability, increased stiffness, and higher temperature applications when compared to unfilled PA.Drop-in replacement for other commercially .. |
|||
Surface Resistance | 2.30e+14 ohm | 2.30e+14 ohm | 50% RH, 500V; ASTM D257 |
ALM PA-615-GS Filled Nylon 12 Prototyping Polymer 50% glass sphere filled material for improved dimensional stability, increased stiffness, and higher temperature applications when compared to unfilled PA.Drop-in replacement for other commercially .. |