Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 2.41e+13 ohm | 2.41e+13 ohm | IEC 60093 |
Vyncolit X7255 Glass Fiber Reinforced Novolac Phenolic Novolac resin based, glass fiber and glass beads reinforced. Very easy to transform in complex shapes. Excellent mechanical and thermal properties. Higher isotropic properties and good dimensional s.. |
|||
Surface Resistance | 2.41e+13 ohm | 2.41e+13 ohm | IEC 60093 |
Vyncolit W5020 Glass Filled Novolac Phenolic Novolac resin based, glass fiber and glass bead reinforced. High dimensional stability and excellent chemical resistance at high temperatures in hydraulic brake fluids. Used in the ABS system.Inform.. |