Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 2.50e+15 ohm | 2.50e+15 ohm | ASTM D257 |
Solvay Specialty Polymers Amodel® AT-5001 Polyphthalamide (PPA) Resin, at 50% RH
(discontinued **) AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properti.. |