Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 2.70e+14 ohm | 2.70e+14 ohm | Cond. C |
Abatron AboCast/AboCure 8502-1 Epoxy AboCast/AboCure 8502-1 is a solventless clear Epoxy System, used as a casting, adhesive, and impregnating resin for transformers, capacitors, coils, and other electronic components requiring a low-v.. |