Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 2.78e+15 ohm | 2.78e+15 ohm | IEC 60093 |
Gromax 1163LL TPE 163LL is medium modulus grade with nominal Durometer hardness of 63D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ext.. |