Polymer Property : Surface Resistance = 2.78e+15 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 2.78e+15 ohm
2.78e+15 ohm
IEC 60093
Gromax 1163LL TPE
163LL is medium modulus grade with nominal Durometer hardness of 63D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ext..