Polymer Property : Surface Resistance = 3.00e+13 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 3.00e+13 ohm
3.00e+13 ohm
Z direction; C96/35/90; ASTM D257
Rogers Corporation RT/duroid® 5880 Glass Microfiber Reinforced PTFE High Frequency Laminate
RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to..
Surface Resistance 3.00e+13 ohm
3.00e+13 ohm
IEC 60093
Solvay TECHNYL® B 218L V20 Black 44 N PA66, 25% glass fiber, DRY
Description: Copolyamide 66/6, reinforced with 20% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistanceAvailable in: Asia Pacific and EuropeProduct Applications:..
Surface Resistance 3.00e+13 ohm
3.00e+13 ohm
IEC 60093
Solvay TECHNYL® B 218L V30 Black 44 N PA66, 30% glass fiber, DRY
Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistance.Available in: Asia Pacific, Europe and Latin AmericaProdu..
Surface Resistance 3.00e+13 ohm
3.00e+13 ohm
ROA; IEC 60093
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Surface Resistance 3.00e+13 ohm
3.00e+13 ohm
ROA; IEC 60093
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Europe-Africa-Middle East)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
Surface Resistance 3.00e+13 - 5.00e+13 ohm
3.00e+13 - 5.00e+13 ohm
ROA; IEC 60093
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS
Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a..
Surface Resistance 3.00e+13 - 5.00e+13 ohm
3.00e+13 - 5.00e+13 ohm
ROA; IEC 60093
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS (Asia Pacific)
Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a..
Surface Resistance 3.00e+13 ohm
3.00e+13 ohm
ROA; IEC 60093
SABIC Innovative Plastics Ultem ATX152R PEI+PCE
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Surface Resistance 3.00e+13 ohm
3.00e+13 ohm
IEC 60093
Polyplastics Duranex® 6302T Polybutylene Terephthalate (PBT), Low friction, Low wear, Mineral filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Surface Resistance 3.00e+13 ohm
3.00e+13 ohm
IEC 60093
Polyplastics Duracon® SX-35 Acetal Co-polymer (POM), Flexible, Lower noise
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Surface Resistance 3.00e+13 ohm
3.00e+13 ohm
cond; IEC 60093
DSM Novamid® 1013G45 1 NA PA6-GF45
45% Glass Reinforced, Injection Molding
Surface Resistance 3.00e+13 ohm
3.00e+13 ohm
cond; IEC 60093
DSM Novamid® 1013GH45 1 NA/BK701 PA6-GF45
45% Glass Reinforced, Heat Stabilized, Injection Molding
Surface Resistance 3.00e+13 ohm
3.00e+13 ohm
cond; IEC 60093
DSM Novamid® 1015G35 NAT PA6-GF35
35% Glass Reinforced, Injection Molding
Surface Resistance 3.00e+13 ohm
3.00e+13 ohm
cond; IEC 60093
DSM Novamid® 1015GH35 BK37 PA6-GF35
35% Glass Reinforced, Heat Stabilized, Injection Molding
Surface Resistance 3.00e+13 ohm
3.00e+13 ohm
cond; IEC 60093
DSM Novamid® ST120 NAT PA6-I
Impact Modified, Injection Molding
Surface Resistance 3.00e+13 ohm
3.00e+13 ohm
cond; IEC 60093
DSM Novamid® ST220 NAT PA6-I
Impact Modified, Injection Molding, Medium Viscosity
Surface Resistance 3.00e+13 ohm
3.00e+13 ohm
C96/35/90; IPC TM-650 2.5.17.1
Arlon MULTICLAD™ HF Halogen-Free Low-Loss Laminate and Prepreg System
MULTICLAD™ HF represents the next generation low-loss thermoset and prepreg system for high-speed and high-frequency printed circuit boards. This technology combines a low-loss, high reliability t..